§154.605. Toughness test.
46 C.F.R. § 154.605
Each toughness test under §§ 154.610 through 154.625 must meet Subpart 54.05 of this chapter.
If subsize test specimens are used for the Charpy V-notch toughness test, the Charpy V-notch energy must meet Table 54.05-20 (a) of this chapter.
Notes, amendments, and revision history
Authority
Authority: 46 U.S.C. 3703, 9101; Department of Homeland Security Delegation No. 0170.1.
Source
Source: CGD 74-289, 44 FR 26009, May 3, 1979, unless otherwise noted.