# §195.114. Used pipe.


Any used pipe installed in a pipeline system must comply with § [195.112 (a)](/cfr/49/195.112.md?p=a) and [(b)](/cfr/49/195.112.md?p=b) and the following:

- (a) The pipe must be of a known specification and the seam joint factor must be determined in accordance with [§ 195.106(e)](/cfr/49/195.106.md?p=e). If the specified minimum yield strength or the wall thickness is not known, it is determined in accordance with § [195.106 (b)](/cfr/49/195.106.md?p=b) or [(c)](/cfr/49/195.106.md?p=c) as appropriate.
- (b) There may not be any:
  - (1) Buckles;
  - (2) Cracks, grooves, gouges, dents, or other surface defects that exceed the maximum depth of such a defect permitted by the specification to which the pipe was manufactured; or
  - (3) Corroded areas where the remaining wall thickness is less than the minimum thickness required by the tolerances in the specification to which the pipe was manufactured.

## Notes

### Amendments

[Amdt. 195-22, 46 FR 38360, July 27, 1981; 47 FR 32721, July 29, 1982]

### Authority

Authority: 30 U.S.C. 185(w)(3), 49 U.S.C. 5103, 60101 et seq., and 49 CFR 1.97.

### Source

Source: Amdt. 195-22, 46 FR 38360, July 27, 1981, unless otherwise noted.